Steel Structure

Welding Procedure Specification for Steel Structures

Welding Procedure Specification (WPS) for Steel Structures

A Welding Procedure Specification (WPS) is a documented set of parameters that tells welders exactly how to join a given material. Without a qualified WPS, weld quality depends on individual habit rather than controlled process.

What a WPS Covers

Item Purpose
Base metal and thickness range Defines what the procedure is qualified for
Filler metal Electrode or wire type and size
Welding current and voltage Controls penetration and heat input
Preheat and interpass temperature Prevents cracking in thick sections
Welding position Flat, horizontal, vertical or overhead
Joint design and technique Groove, fillet, pass sequence
Inspection requirements Visual, UT or MT acceptance

Welder Qualification

Each welder must be qualified for the position and thickness they work on, normally through a procedure qualification record (PQR) and a welder performance test. Certificates should be traceable to the specific joint type.

  • Check welder ID stamps on completed welds.
  • Confirm current qualification certificates are valid.
  • Match qualification thickness to production thickness.

Common Defects and Prevention

  1. Porosity: caused by damp electrodes or dirty surfaces; pre-dry and clean.
  2. Undercut: too high current or wrong travel speed; adjust parameters.
  3. Cracking: lack of preheat in thick sections; follow the WPS preheat range.
  4. Incomplete penetration: insufficient root gap or current.

Why Buyers Should Ask for the WPS

A factory that can produce a qualified WPS and matching inspection reports is far more reliable than one that welds purely by experience. Ask for the WPS, PQR and welder certificates before shipment.

See our crane workshop design guide or request welding documentation.